Do you have fusing and annealing temps for 104 coe

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
lorwolff
Posts: 22
Joined: Sun Apr 19, 2009 5:37 pm
Location: Keyport and Seattle, Washington

Do you have fusing and annealing temps for 104 coe

Post by lorwolff »

I have lost my notes for firing Effetre soft glass.
I would like to try something with rods and murrini, but do not remember the full fuse temp, or best annealing tempurature.

Has anyone here done fusing with this mainly bead making glass?
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Do you have fusing and annealing temps for 104 coe

Post by Stephen Richard »

Here is a table from Kirwan that might be useful
http://glasstips.blogspot.co.uk/2010/07 ... fetre.html
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/