Has anyone used George's Rigidizer? It is a blue-green liquid. I coated 1/8 inch fiber with it but noticed the back was still white. Should I coat the back as well? There was no instructions for pre-firing it.

Thanks,

Dave
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: George's Rigidizer

Post by rosanna gusler »

i would coat both sides. Fire to whatever temp you are going to use it at kiln wash and use .rosannat
artist, owner of wanchese art studio, marine finisher
dkingman
Posts: 3
Joined: Sun Feb 12, 2006 11:34 am
Location: Eugene, OR
Contact:

Re: George's Rigidizer

Post by dkingman »

Thanks Rosanna
Post Reply