I had a good friend ask about making a strip bowl with a Navajo style pattern. This is what I ended up with. Just finished the edges and it goes in for slump this afternoon.
Tim Yardic
Yardic Glassworks
Yardic Glassworks
-
- Posts: 308
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Navajo
Fantastic work!
Jim
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Re: Navajo
Saw it on your FB page. Looks awesome!
-
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Navajo
Ditto the above comments: WOW!
-
- Posts: 215
- Joined: Mon Mar 10, 2003 1:01 pm
- Location: Salt Spring Island, British Columbia
- Contact:
Re: Navajo
Great work Tim,
I enlarged the image and saw that your lines are perfectly aligned and symmetrical. Incredible detail.
Cheers,
Bob
I enlarged the image and saw that your lines are perfectly aligned and symmetrical. Incredible detail.
Cheers,
Bob
Re: Navajo
An absolutely gorgeous piece! Very impressive craftsmanship! Congratulations!
-
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
-
- Posts: 28
- Joined: Sat Sep 01, 2007 11:49 pm
- Location: Central Coast of California
Re: Navajo
This is beautiful!!
Barb
Barb
Re: Navajo
Beautiful piece, you must have been there hrs to line up those sharp line
Nice work
Nice work
-
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Navajo
Great job, your friend will be happy.
Bob
Bob
-
- Posts: 71
- Joined: Tue Sep 21, 2004 11:10 pm
- Location: Massachusetts
- Contact:
Re: Navajo
Is that white and clear in those subtle stripes? This is very well done!
-
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Navajo
Survived the slump and now you can better see the edges. Someone asked about clear strips; There is no clear in this bowl. The lighter colors are Ivory and Almond. Thanks, Tim
Tim Yardic
Yardic Glassworks
Yardic Glassworks
-
- Posts: 3
- Joined: Sat Dec 02, 2006 6:33 pm
- Location: Chandler, Az
- Contact:
Re: Navajo
That is a beautiful bowl. Did you find the pattern online or create it yourself? Your work shows perfection!
Brad Peterson
http://www.bradpetersonsglassart.com
http://www.bradpetersonsglassart.com
-
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Navajo
Brad,
I reviewed patterns on a number of Navajo blankets and found some common themes throughout, such as the zig zag, then drew my own pattern which resulted in this piece. If you go to The Glass Hole Facebook page you can see photos of the build. Thanks for your nice comments. Tim
I reviewed patterns on a number of Navajo blankets and found some common themes throughout, such as the zig zag, then drew my own pattern which resulted in this piece. If you go to The Glass Hole Facebook page you can see photos of the build. Thanks for your nice comments. Tim
Tim Yardic
Yardic Glassworks
Yardic Glassworks
-
- Posts: 18
- Joined: Sun Apr 25, 2004 2:43 pm
- Location: Wilmington, NC
- Contact:
Re: Navajo
Beautiful work.
-
- Posts: 308
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Navajo
Anyplace else that I can view the build besides Facebook? I don't "like" Facebook.
Jim
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Re: Navajo
Wonderfully precise; I very much like the way you've captured the "blanket" quality.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)