Low firing schedule

Post by Sherry R »

I'm trying to make snowflakes and the mold I'm using calls for a low fire schedule. I'm using 96 and the schedule I found is
500 - 1200 - 15
500 - 1400 - 5
9999 - 960 - 60
Would this schedule be what I want?
haleybach
Posts: 75
Joined: Tue Sep 04, 2012 1:59 pm
Location: Austin TX

Re: Low firing schedule

Post by haleybach »

I just read a blog post about someone who was using the snowflake mold:

http://idlecreativity.wordpress.com/201 ... onderland/

HTH
Haley