My frit collection is growing, a good thing :wink: I have a kitchen strainer I use like a gold miner to sort medium sized frit, it has perfect sized chicken wire mini holes. Any suggestion for screening that will sort out finer sizes? Traditional window screen just sorts powder...ideas? Tia!
http://www.carasmiths.com
Facebook: Caco CaraSmiths

Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Screening frit

Postby Bert Weiss » Wed Feb 20, 2013 10:01 am

Caco wrote:My frit collection is growing, a good thing :wink: I have a kitchen strainer I use like a gold miner to sort medium sized frit, it has perfect sized chicken wire mini holes. Any suggestion for screening that will sort out finer sizes? Traditional window screen just sorts powder...ideas? Tia!
Screens are made in a complete range of exact sizes from superfine on up. 2 industries that utilize screens are potters and gardeners. I have a set of loam screens I like to use when sorting mid sized frits. They were not expensive. Go on either Bullseye or 96 and see what mesh size they use to grade the frits they sell. Look for those sizes. Google screen mesh sizes to look at charts that show the opening sizes of various screens. Thompson enamel sells finer mesh screens for sifting on frits.

Frits are rated by a range of mesh sizes. So 80/200 would be everything that falls through the 200 and doesn't fall through the 80. This sort of grading will remove fines and yield the best grade of frits. I picked those numbers as an arbitrary pair.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Jeanne
Posts: 75
Joined: Wed Aug 20, 2003 8:16 am
Location: NJ

Re: Screening frit

Postby Jeanne » Wed Feb 20, 2013 10:32 am

I made a simple set of screen sifters. I bought 4 cheap ($1) picture frames at Michaels and hot glued different size screening that I had (largest is 5mm). You could also make some small wood boxes and do the same - but the picture frames were fast. I stack them on top of each other and sift the crushed glass through. What's left on the top I will crush and sift again. (I drag a 2 x 2" piece of glass over the screen to get the fine pieces out of the mesh.) I bought 100s of small 2 oz jars off the web and have them sorted by color. It's very simple and gives me a nice selection of sizes and colors for accenting.

Image

http://imgur.com/ZJdxfX4

Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Screening frit

Postby Peter Angel » Wed Feb 20, 2013 8:07 pm

It bought this frit sorting set and it works very well. I'm sure you can buy something similar locally.

http://glassfusing.com.au/product/glass ... rting-set/
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.

Caco
Posts: 21
Joined: Thu Jun 10, 2010 2:59 pm
Location: Eastern PA
Contact:

Re: Screening frit

Postby Caco » Wed Feb 20, 2013 8:25 pm

Thanks all!

[quote="Jeanne"]I made a simple set of screen sifters. I bought 4 cheap ($1) picture frames at Michaels >>

Jeanne, I was thinkg same as I have a stack of frames and want to mix some home made color combos. Off to Lowes for some screen scraps!
http://www.carasmiths.com
Facebook: Caco CaraSmiths

Michele gh
Posts: 71
Joined: Tue Sep 21, 2004 11:10 pm
Location: Massachusetts
Contact:

Re: Screening frit

Postby Michele gh » Wed Feb 20, 2013 8:42 pm

I was given the Aanraku Frit Sifters. They are a bit pricey to buy, but they are a convenient size and work well.

http://www.aanraku.com/aanraku-frit-sifter.html

S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: Screening frit

Postby S.TImmerman » Sat Feb 23, 2013 2:17 am

Michele gh wrote:I was given the Aanraku Frit Sifters. They are a bit pricey to buy, but they are a convenient size and work well.

http://www.aanraku.com/aanraku-frit-sifter.html

I bought those at D&L art glass for 33.00 -12.00 cheaper

Laurie Saukko
Posts: 13
Joined: Tue Mar 13, 2012 12:57 pm

Re: Screening frit

Postby Laurie Saukko » Fri Mar 08, 2013 1:25 pm

go to the the dollar store. I have a flour sifter that gives me medium frit and they have reusable coffee filters that will screen out the powder...a holey soup ladle will get out your big chunks, mosiac size. works great, you don't have to build anything and all for $3-4 dollars!


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 4 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com