Screening frit
Moderator: Brad Walker
Screening frit
My frit collection is growing, a good thing
I have a kitchen strainer I use like a gold miner to sort medium sized frit, it has perfect sized chicken wire mini holes. Any suggestion for screening that will sort out finer sizes? Traditional window screen just sorts powder...ideas? Tia!
http://www.carasmiths.com
Facebook: Caco CaraSmiths
Facebook: Caco CaraSmiths
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Screening frit
Screens are made in a complete range of exact sizes from superfine on up. 2 industries that utilize screens are potters and gardeners. I have a set of loam screens I like to use when sorting mid sized frits. They were not expensive. Go on either Bullseye or 96 and see what mesh size they use to grade the frits they sell. Look for those sizes. Google screen mesh sizes to look at charts that show the opening sizes of various screens. Thompson enamel sells finer mesh screens for sifting on frits.Caco wrote:My frit collection is growing, a good thingI have a kitchen strainer I use like a gold miner to sort medium sized frit, it has perfect sized chicken wire mini holes. Any suggestion for screening that will sort out finer sizes? Traditional window screen just sorts powder...ideas? Tia!
Frits are rated by a range of mesh sizes. So 80/200 would be everything that falls through the 200 and doesn't fall through the 80. This sort of grading will remove fines and yield the best grade of frits. I picked those numbers as an arbitrary pair.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Screening frit
I made a simple set of screen sifters. I bought 4 cheap ($1) picture frames at Michaels and hot glued different size screening that I had (largest is 5mm). You could also make some small wood boxes and do the same - but the picture frames were fast. I stack them on top of each other and sift the crushed glass through. What's left on the top I will crush and sift again. (I drag a 2 x 2" piece of glass over the screen to get the fine pieces out of the mesh.) I bought 100s of small 2 oz jars off the web and have them sorted by color. It's very simple and gives me a nice selection of sizes and colors for accenting.

http://imgur.com/ZJdxfX4
http://imgur.com/ZJdxfX4
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Screening frit
It bought this frit sorting set and it works very well. I'm sure you can buy something similar locally.
http://glassfusing.com.au/product/glass ... rting-set/
http://glassfusing.com.au/product/glass ... rting-set/
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Re: Screening frit
Thanks all!
[quote="Jeanne"]I made a simple set of screen sifters. I bought 4 cheap ($1) picture frames at Michaels >>
Jeanne, I was thinkg same as I have a stack of frames and want to mix some home made color combos. Off to Lowes for some screen scraps!
[quote="Jeanne"]I made a simple set of screen sifters. I bought 4 cheap ($1) picture frames at Michaels >>
Jeanne, I was thinkg same as I have a stack of frames and want to mix some home made color combos. Off to Lowes for some screen scraps!
http://www.carasmiths.com
Facebook: Caco CaraSmiths
Facebook: Caco CaraSmiths
-
Michele gh
- Posts: 71
- Joined: Tue Sep 21, 2004 11:10 pm
- Location: Massachusetts
- Contact:
Re: Screening frit
I was given the Aanraku Frit Sifters. They are a bit pricey to buy, but they are a convenient size and work well.
http://www.aanraku.com/aanraku-frit-sifter.html
http://www.aanraku.com/aanraku-frit-sifter.html
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: Screening frit
I bought those at D&L art glass for 33.00 -12.00 cheaperMichele gh wrote:I was given the Aanraku Frit Sifters. They are a bit pricey to buy, but they are a convenient size and work well.
http://www.aanraku.com/aanraku-frit-sifter.html
-
Laurie Saukko
- Posts: 13
- Joined: Tue Mar 13, 2012 12:57 pm
Re: Screening frit
go to the the dollar store. I have a flour sifter that gives me medium frit and they have reusable coffee filters that will screen out the powder...a holey soup ladle will get out your big chunks, mosiac size. works great, you don't have to build anything and all for $3-4 dollars!