Postby Studiodunn » Wed Feb 27, 2013 8:54 am

Greetings All!

Today I am planning on signing my Magless pieces and getting them into the mail! Yeehaw! However I could use a little advice before I do so. My plan is to dremel etch my signature on the back of each piece. The base glass is white which will make it difficult to see the etching. What can I rub over the signature to make it stand out better?

Thank you!
“I would rather die than hate you.”
- Martin Luther King

Nicole Hanna
Posts: 27
Joined: Wed Jul 27, 2005 10:17 am
Location: SW Missouri
Contact:

Re: Signing work for Magless

Postby Nicole Hanna » Wed Feb 27, 2013 10:50 am

I usually just go over it with a black marker, then wipe off the excess.
When I stand before God at the end of my life, I would hope that I would have not a single bit of talent left and could say, "I used everything you gave me." (erma bombeck)

Jeanne
Posts: 75
Joined: Wed Aug 20, 2003 8:16 am
Location: NJ

Re: Signing work for Magless

Postby Jeanne » Wed Feb 27, 2013 11:20 am

I use a 2mm barrel shaped diamond coated bit to sign my pieces. You can see that on it's own. Some other diamond coated bits I have (the pointy ones) are too fine and don't show up very well.

Barry Kaiser
Posts: 285
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Signing work for Magless

Postby Barry Kaiser » Wed Feb 27, 2013 1:19 pm

Try the Harbor freight engraving pen. It has a small ball bit and works like a charm.
\


Barry

RachelM
Posts: 47
Joined: Mon Oct 24, 2011 11:26 pm

Re: Signing work for Magless

Postby RachelM » Fri Mar 01, 2013 11:44 am

I like Barry's idea since I got one of these engraving pens from Harbor Freight for a holiday gift from someone!
And,the back of my magless(es?) are also white.


Rachel :)
imaglassydiva@aol.com

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Signing work for Magless

Postby bob proulx » Fri Mar 01, 2013 12:06 pm


Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Signing work for Magless

Postby Kevin Midgley » Fri Mar 01, 2013 3:14 pm

shoe polish rubbed in engraved area.

Studiodunn
Posts: 106
Joined: Sun Sep 11, 2011 9:30 am
Location: The Dunn-Inn
Contact:

Re: Signing work for Magless

Postby Studiodunn » Fri Mar 01, 2013 4:00 pm

Lots of excellent ideas for future reference...

Before I shipped them on Wed., I tried black sharpie on a sample and discovered I could ever so slightly see it when light was able to shine through the piece. So for this batch, I just left the etched signature without color. But I appreciate knowing other options to consider for future projects!

Thank you!
“I would rather die than hate you.”
- Martin Luther King

Al Bray
Posts: 42
Joined: Thu May 01, 2003 8:37 pm
Location: Lansing, Michigan
Contact:

Re: Signing work for Magless

Postby Al Bray » Mon Mar 04, 2013 11:43 am

Studiodunn wrote:Lots of excellent ideas for future reference...

Before I shipped them on Wed., I tried black sharpie on a sample and discovered I could ever so slightly see it when light was able to shine through the piece. So for this batch, I just left the etched signature without color. But I appreciate knowing other options to consider for future projects!

Thank you!


I just ordered one of these as I had to order a gold coated face shield from Wale Apparatus and I noticed them when looking over their other product offerings:

http://www.waleapparatus.com/catalog.as ... prevnext=1

Not sure how it is going to work especially on darker colored opals or transparent glass, but I like the idea of how it works from the description and I will follow up after I have had a chance to give it a try.

- Al

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Signing work for Magless

Postby bob proulx » Mon Mar 04, 2013 12:56 pm

Al Bray wrote:
Studiodunn wrote:Lots of excellent ideas for future reference...

Before I shipped them on Wed., I tried black sharpie on a sample and discovered I could ever so slightly see it when light was able to shine through the piece. So for this batch, I just left the etched signature without color. But I appreciate knowing other options to consider for future projects!

Thank you!


I just ordered one of these as I had to order a gold coated face shield from Wale Apparatus and I noticed them when looking over their other product offerings:

http://www.waleapparatus.com/catalog.as ... prevnext=1

Not sure how it is going to work especially on darker colored opals or transparent glass, but I like the idea of how it works from the description and I will follow up after I have had a chance to give it a try.

- Al

Hi Al, I am a member on a lampworking forum and a lot of people there use this tool and highly recommend it.
Bob


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron