Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

nipping thick murrini

Postby Cheryl » Tue Mar 26, 2013 8:32 pm

Is there such a thing as a mosaic nipper with a bigger opening? I have leponitt (sp?) nippers with great blades, but they are limited in the size that I can cut. Sometimes I get wonderful vitrigraph cane that's about 1/2-7/8 inches thick. The tile saw just eats it (plus it's no fun to hold it to the blade). Ideas welcome...
"Every artist was first an amateur."

--Ralph Waldo Emerson

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: nipping thick murrini

Postby Morganica » Tue Mar 26, 2013 9:42 pm

Well, I do it with the aid of a hammer, like this http://www.morganica.com/bloggery/2011/latest/making-murrini-cane-in-a-kiln-jellyrolls/
Image
It works pretty well and once you get the hang of it is reasonably accurate.

You can also buy murrini guillotines, but they're expensive. This one, by Carlo Dona, is something like $2,500, or was the last time I checked about two years ago:
Image
$2500 buys a lot of cheap choppers and hammers... ;-)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: nipping thick murrini

Postby Cheryl » Tue Mar 26, 2013 10:59 pm

I can't always get my nippers around the cane....

2500. wow. That's insane!
"Every artist was first an amateur."



--Ralph Waldo Emerson

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: nipping thick murrini

Postby Morganica » Tue Mar 26, 2013 11:38 pm

Get bigger nippers...some of them open to an inch or more.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Tom Fuhrman
Posts: 175
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: nipping thick murrini

Postby Tom Fuhrman » Wed Mar 27, 2013 6:28 am

get a very thin and small blade for your tile saw. I got mine from www.lopacki.com , 4" dia. and very thin, use lots of water and go slow, even buy several and make a motor with multiple blades and cut several slices with one pass. little wasteage to rod with this setup.

Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: nipping thick murrini

Postby Cheryl » Wed Mar 27, 2013 7:04 pm

any mfrs on those bigger jawed nippers? Tx
"Every artist was first an amateur."



--Ralph Waldo Emerson

williamslaybaugh
Posts: 30
Joined: Mon Mar 12, 2012 9:07 am
Location: San Diego

Re: nipping thick murrini

Postby williamslaybaugh » Wed Mar 27, 2013 11:30 pm

You could also try a color bar cutter for blown glass. I have not used this model, and most take a bit of practice to get a good brake. They will handle a good thickness of glass though.

http://www.glasscolor.com/products/defa ... 0&pID=1570

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: nipping thick murrini

Postby Tony Smith » Thu Mar 28, 2013 5:10 am

You could make a tool like this
http://hobbyglass.com/Murrini-Chopper-P458592.aspx

The arbor press can be bought from Enco for $40. Then you need someone to weld cutters onto the arbor and table.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: nipping thick murrini

Postby Cheryl » Fri Mar 29, 2013 10:30 pm

...I could....but I don't have ready access to welding and frankly I am feeling a bit lazy on this. Unless you're volunteering? [-o<
"Every artist was first an amateur."



--Ralph Waldo Emerson

RHunter
Posts: 19
Joined: Tue Jan 24, 2006 8:44 pm
Location: Honolulu, Hawaii

Re: nipping thick murrini

Postby RHunter » Sat Mar 30, 2013 5:04 am

Hi All,

A woman that was in my glass class , had picked up a pair of regular tile nippers from Lowe's or Home Depot....they opened wider than the glass nippers we use, and were pretty sweet...they might be just the ticket for larger cane.....glass blowers must have something similar to cut their canes.

Randy

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: nipping thick murrini

Postby Morganica » Sat Mar 30, 2013 12:20 pm

Cheryl wrote:any mfrs on those bigger jawed nippers? Tx

As Randy says, look at tile nippers at hardware stores. Mine (not the wheeled nippers in the photo, but rather straight-bladed jaws) open to about an inch and a quarter.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: nipping thick murrini

Postby Valerie Adams » Sat Mar 30, 2013 4:34 pm

I was just in my local Home Depot and they didn't have anything that opened more than 1/2". I'll continue to search.

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: nipping thick murrini

Postby Tony Smith » Sat Mar 30, 2013 4:45 pm

Cheryl,

Channelock makes nail cutters that open pretty wide... about an inch, but not more than a half inch deep. Home Depot has them. Sneak in a piece of your murrini in and see if they'll work.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

Tom Fuhrman
Posts: 175
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: nipping thick murrini

Postby Tom Fuhrman » Sun Mar 31, 2013 3:54 am

Starrett makes some very good nippers with replaceable blades but they are quite expensive. $100+ if I recall, but very good.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 34 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com