Blade or Wheel Stiffener

Postby Jeanne » Thu Apr 11, 2013 10:58 am

I bought a 6" X .012 saw blade for my 7" Rigid Saw. It needs stabilizing. I see people use 6" stabilizers for 10" blades and I'm wondering if anyone has used 4" stabilizers for a 6" blade? Or... if there's another alternative. Couldn't find any on HIS but saw them on Amazon.

Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Blade or Wheel Stiffener

Postby Rick Wilton » Thu Apr 11, 2013 1:33 pm

I wouldn't think you'd need a stabilizer on a small blade like 6" you shouldn't get too much flex out of that size blade. A four inch stabilizer on a 6" blade will leave you maybe 1/2" to 3/4" of usable cutting depth.

Why do you think you need a stabilizer?
Rick Wilton

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Blade or Wheel Stiffener

Postby Kevin Midgley » Thu Apr 11, 2013 1:40 pm

oh Rick you can get flex alright on a small blade. Been there done that. Lapidary thin blades can sure save on kerf width loss but you really have to treat them right or they can be permanently distorted pretty quick.
So yes with a blade that thin, get the stiffeners. You've been warned.

Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Blade or Wheel Stiffener

Postby Rick Wilton » Thu Apr 11, 2013 5:23 pm

Kevin, I've never used a 6" blade so I'll yield to your judgement on that, however I think a 4" stiffener may be problematic as that'll leave only 1 inch of blade exposed which would leave you 3/4" max cutting depth.
Rick Wilton

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Blade or Wheel Stiffener

Postby Kevin Midgley » Thu Apr 11, 2013 5:51 pm

Absolutely correct Rick about the cutting depth but with a really skinny blade anything not perfect in the cutting process results in a bent useless blade.

Cheryl
Posts: 239
Joined: Sun Mar 09, 2003 7:56 pm
Location: Tallahassee FL
Contact:

Re: Blade or Wheel Stiffener

Postby Cheryl » Thu Apr 11, 2013 6:00 pm

Give H.I.S. a call. They may have them even tho not on the web site. Plus they'll give you great advice!
"Every artist was first an amateur."

--Ralph Waldo Emerson


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 56 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com