Postby susanmozingo » Sat May 18, 2013 11:24 am

Do they have a shelf life? Thank you

Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Glastac and Klyr-Fire

Postby Stephen Richard » Sat May 18, 2013 4:50 pm

not to my knowledge
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Glastac and Klyr-Fire

Postby Bert Weiss » Sun May 19, 2013 8:06 am

I think any organic liquid can get moldy and funky. The other side of the coin is that I don't think this is much of a problem for most places. I would not be surprised to hear that people who live in damp moldy places, have more problems than people in most other climates. I have kept containers of liquid CMC around for years with no problems. Come to think about it, I once got a spray medium (CMC is the primary ingredient) sent to me in a metal can. That can rusted terribly and killed the medium. The same stuff in a plastic container is good, though.

I don't know the formula for Glasstac. Klyrfire is a 3% solution of CMC. Glasstac has more.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Glastac and Klyr-Fire

Postby Peter Angel » Mon May 20, 2013 7:11 pm

Bert Weiss wrote:
Klyrfire is a 3% solution of CMC.


Bert, do you know what the other 97% is made of?

Peter
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Glastac and Klyr-Fire

Postby Brock » Mon May 20, 2013 7:18 pm

Google. If you type Klyr-Fire MSDS into it, you'll find out . . .

RHunter
Posts: 19
Joined: Tue Jan 24, 2006 8:44 pm
Location: Honolulu, Hawaii

Re: Glastac and Klyr-Fire

Postby RHunter » Wed May 22, 2013 12:17 pm

Hi All,

I think there may be different formulations of CMC. I bought a container of cmc in japan and upon making a batch , it would go moldy within a couple of weeks....which kind of put me off using it as a glue for laying up projects....now here in the US, I bought some from my ceramic supplier which has lasted for several months... So my edumacated guess is there are different grades or purities....further from what I know , Japan is sort of opposed to additives, nitrates etc...so maybe their CMC is more pure and doesn't contain mold inhibitors or extenders. Another possibility is the minerals of the tap water, along with a previous poster's suggestion that climate may play a part.

Randy

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Glastac and Klyr-Fire

Postby Morganica » Wed May 22, 2013 1:28 pm

Climate, the water you're using, the container you're using, how long it's open and what happens to be floating by while it's open, if the window's open when you're mixing it up, if there's mold in your studio, all kinds of things. I think the CMC powder I buy has nothing but CMC, and sometimes a batch gets moldy, sometimes it doesn't.

I find I get more life out of a batch if I use a sterilized container, i.e. I boil it the way I would canning jars. Less trouble to simply add a drop of bleach to the mix, and use no more than I'll be needing for a couple of weeks.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Glastac and Klyr-Fire

Postby Bert Weiss » Wed May 22, 2013 4:06 pm

I wonder if methyl cellulose is a short term for carboxymethylcellulose, or are they different? I tend to think they are the same.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions

RHunter
Posts: 19
Joined: Tue Jan 24, 2006 8:44 pm
Location: Honolulu, Hawaii

Re: Glastac and Klyr-Fire

Postby RHunter » Wed May 22, 2013 5:12 pm

Hi All,

Wikipedia , written by someone(s) with way more insight than me, seems to reference several variations of CMC so it seems to be luck of the draw, as to what we buy and where we buy it and then how it behaves once we mess with it.

http://en.wikipedia.org/wiki/Carboxymethyl_cellulose

Randy

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Glastac and Klyr-Fire

Postby Kevin Midgley » Wed May 22, 2013 6:24 pm

There's food grade and 'other'.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com