Hi All,
I dislike coating molds, and kiln shelves, with a Hake Brush....orthodoxy says use one.....without ever explaining why.....nor how to avoid the endless shedding these things put out, much like a long haired dog.
Questioning Authority leads me to ask, WHY ?
I understand from Googling other site sources that Hake Brushes hold a boatload of water, which gives good results puddling kiln wash, onto said mold or kiln shelf, also their fine-ness prevents dislodging previous layers of material as multiple layers are needed to effectively coat a shelf or mold.
I wonder if back in the day , this was a good cheap solution to getting good coverage without crumbling off the previous layer on successive coatings.
Does anyone know of a technologically advanced manual alternative ( thus not air brush, etc ) be it a type of paint brush , or alternative method that would accomplish this task without endless holidays and the requisite picking out of stray hairs....maybe I should just use a long haired dog though that would introduce a whole new set of problems , what with squirming and all. <G>
There are endless varieties of these type brushes available in Japan, and they are used to paint with....(houses) and for the life of me I don't know how they manage....
thanks,
Randy
Hake Brushes
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Hake Brushes
You can spray it on with a mouth atomizer or it's automated cousin the Paasche 62 sprayer.
The mouth atomizer is what I call " a cheap thrill."
The mouth atomizer is what I call " a cheap thrill."
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Hake Brushes
They manage because they use high quality brushes. Really, most of the brushes we get are inferior.
You can spray batt wash on with a mouth atomiser if you like. Need to mix the separator more thinly, and so apply more coats. But it works
You can spray batt wash on with a mouth atomiser if you like. Need to mix the separator more thinly, and so apply more coats. But it works
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Hake Brushes
If they are falling out in the store then they aren't the ones you want to use. Try a pottery supply place and pay the premium. Synthetics will work but if you like to apply the wash to a pre-warmed shelf, they may just melt and cause other problems.
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Hake Brushes
Potters use Hake brushes to brush transparent glaze onto bisqued fired ceramics.
They trim the hake brush bristles down to 1/2 the original length.
You could use sharp scissors or a sharp blade to trim the bristles.
I'm planing to try this soon and I will let you know the results.
Pete
They trim the hake brush bristles down to 1/2 the original length.
You could use sharp scissors or a sharp blade to trim the bristles.
I'm planing to try this soon and I will let you know the results.
Pete
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Hake Brushes
I use a high quality paint brush for all my shelves and molds. Works great with no shedding.
Tim Yardic
Yardic Glassworks
Yardic Glassworks
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Hake Brushes
I use the cheap foam brushs you buy at any hardware store and they work fine. Leave them in the kiln wash and they last a long time. Which ever brush you use if you want a smoother finish on the shelf use an old pair of nylons and rub lightly.
Bob
Bob
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Hake Brushes
I used to use a small paint roller to apply wash to shelves.
Then I switched to spraying on with a garden sprayer.
(With both methods, I needed to smooth the wash a bit when it was dry.)
In past years I've gone back to the brush, deciding it's simpler. I simply wipe off the few stray hairs when the wash is dry.
Then I switched to spraying on with a garden sprayer.
(With both methods, I needed to smooth the wash a bit when it was dry.)
In past years I've gone back to the brush, deciding it's simpler. I simply wipe off the few stray hairs when the wash is dry.