Element placement and firing results

Post by Chelseaglass »

I just purchased a Caldera to have a travel kiln. Realizing it probably takes a few experimental runs, will there be much difference in firing from a Fusion 16 with a top/lid element, vs the side elements in this small kiln? I plan to fuse 6x6 tiles.

chelseaglass
Arnold Howard
Posts: 47
Joined: Mon Oct 13, 2003 5:21 pm
Location: Converse, Texas USA
Contact:

Re: Element placement and firing results

Post by Arnold Howard »

Chelseaglass wrote:I just purchased a Caldera to have a travel kiln. Realizing it probably takes a few experimental runs, will there be much difference in firing from a Fusion 16 with a top/lid element, vs the side elements in this small kiln? I plan to fuse 6x6 tiles.

chelseaglass
Thank you for your business. If you fire with full rates, you will notice that the Caldera fires much faster than the Fusion-16.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / http://www.paragonweb.com