Can CoreLite kiln shelves be used with glass? Are they easy to cut if the size needs to be trimmed down from a larger shelf?

Tracy Fries
Posts: 41
Joined: Thu Jun 14, 2012 7:14 pm

Re: CoreLite Kiln Shelves

Postby Tracy Fries » Sat Aug 17, 2013 12:18 am

I use them. I purchased from Seattle Pottery and they happily cut them to size before shipping.

Brad Walker
Site Admin
Posts: 1363
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: CoreLite Kiln Shelves

Postby Brad Walker » Sat Aug 17, 2013 8:34 am

Nbolinger wrote:Can CoreLite kiln shelves be used with glass? Are they easy to cut if the size needs to be trimmed down from a larger shelf?


They work fine with glass and can be cut with a tile saw just like a regular mullite/cordierite shelf. It's better if you cut across the hollow pockets, rather than parallel to them.

pgegen
Posts: 1
Joined: Thu Sep 08, 2005 11:56 pm
Location: Wichita, KS

Re: CoreLite Kiln Shelves

Postby pgegen » Sun Aug 18, 2013 11:23 pm

Corelite shelves work fine for glass. The lighter weight is a real plus.

Just a reminder, the recommended heating and/or cooling rate for corelite shelves is only 200 degrees per hour.

dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Re: CoreLite Kiln Shelves

Postby dee » Sun Aug 18, 2013 11:31 pm

i have corelite kiln shelves for my "papa" kiln and love them! i do ramp up 366 dph on initial firings and 250 dph for slump firings w/o a problem.
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com

Yardic Glassworks
Posts: 80
Joined: Sat Mar 06, 2010 9:29 am

Re: CoreLite Kiln Shelves

Postby Yardic Glassworks » Mon Aug 19, 2013 9:06 pm

I have 3 that I use consistently. I have found that they do not like pot melts, but I love them for everything else.
Tim Yardic
Yardic Glassworks


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 43 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com