Bevel edges of glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Judy W
Posts: 8
Joined: Wed Feb 15, 2006 1:42 am

Bevel edges of glass

Post by Judy W »

My piece of glass won't fit into 1/4" lead channel. What is the best way to bevel the edges so it will?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Bevel edges of glass

Post by Kevin Midgley »

JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Bevel edges of glass

Post by JestersBaubles »

A bevel or ripple bit for your grinder:

http://www.sunshineglass.com/rcol/c-too ... c-bits.htm

Dana W.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Bevel edges of glass

Post by Marty »

Or lift the leaf of the came with your fid.