adjusting sheet glass to fit my needs - WarmGlass.com

adjusting sheet glass to fit my needs

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

adjusting sheet glass to fit my needs

Postby KaCe » Fri May 02, 2014 7:09 am

Is there a name for a process that uses frit on a base sheet of glass to get a color that you want to use in a piece? I want to look up firing schedules/color combos/etc. but don't know if it has a specific name. I was thinking of making frit balls and putting them in a pattern on some glass and firing them into the sheet. Then using that sheet in a piece of work. I was also considering sprinkling frit powder over a neutral base sheet and firing. Any direction on this is very welcomed.

Thank you. KaCe

Don Burt
Posts: 537
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: adjusting sheet glass to fit my needs

Postby Don Burt » Fri May 02, 2014 8:43 am

That's why the frit is sold. That's what people do. 'Painting with light' is the appropriated marketing phrase. There are courses galore. And some pretty good bulletin boards.

KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: adjusting sheet glass to fit my needs

Postby KaCe » Fri May 02, 2014 6:02 pm

Thank you, Don. I know people paint with frit. I know that people make patterns with it. I just wasn't sure what a single sheet of glass with frit on it was called if the purpose was merely to change the color/pattern for future work. Thank you. Could you tell me if I'm using 3mm sheet glass should I just tac fuse it, or will that hot still shrink the glass up to thicker glass? Or am I all wet? Should I be thinking of 6mm thick glass and not try to make thinner sheets? Hmm, I had never thought of the issue of keep a sheet thin before.

Since my daughter's brain cancer is over I can now actually work on glass. I had so many false starts prior to this year. I am excited to actually be making work. I only wish that the wonderful class I took from Avery was just a few months ago, instead of years ago. <shrug> Oh, well, onward!

KaCe
Last edited by KaCe on Fri May 02, 2014 6:03 pm, edited 1 time in total.

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: adjusting sheet glass to fit my needs

Postby Morganica » Fri May 02, 2014 6:02 pm

Yup. It's not hard to do and it gets you exactly what you want. It's also called making "part sheets," and it's an extremely useful technique. My mom wanted glass with a friend's favorite colors when she was making her a Christmas present, so we did exactly that:
http://www.morganica.com/bloggery/2006/glasswork/fusingtack-fusing/moms-making-her-own-glass/

About the only caveat I'd add is that when you're working with single sheets (i.e., only 2-3mm thick), you need to control the amount of heatwork you're putting into the glass a bit more than with 6mm-plus layups, to avoid thinning it out too much and/or causing holes. And even then, a single-layer, full-fused sheet will dogbone a bit (i.e., pull in at the center edges) and lip (form a slightly thickened, rounded-over edge).

I get around that by making the part sheet at least an inch bigger, both ways, than the finished size I'll need. Then I simply trim off the distorted areas.

I think, if you're a Bullseye video subscriber, there's a tutorial on how this is done.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: adjusting sheet glass to fit my needs

Postby KaCe » Fri May 02, 2014 6:10 pm

Cynthia,
Yes, I am a subscriber. So I'll look up "part sheets". Thank you for the link and the advise. I have set an ambitious goal of having 8 piece for a series done by the end of May. I was just approached about donating to an auction. I'm not quite sure how I feel about that. As the donated pieces won't put money in my pocket, but it will get my work seen, but then pricing is a question too. I think I'll take this aspect to a different topic area.

You are always so spot-on with your advise. Thank you. Oh, I did get squared away with Dawn detergent and boraxo cleanser. My devit is less and less, but I had to fire one piece five times... I had to sandblast it four times to remove devit, a thumbprint and some soapy scum from under frit balls. I will trod much more carefully when cleaning my work now that I've had to work so hard to correct my errors.

Thanks again..
KaCe

Don Burt
Posts: 537
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: adjusting sheet glass to fit my needs

Postby Don Burt » Fri May 02, 2014 10:54 pm

KaCe wrote:Thank you, Don. I know people paint with frit. I know that people make patterns with it. I just wasn't sure what a single sheet of glass with frit on it was called if the purpose was merely to change the color/pattern for future work. Thank you. Could you tell me if I'm using 3mm sheet glass should I just tac fuse it, or will that hot still shrink the glass up to thicker glass? Or am I all wet? Should I be thinking of 6mm thick glass and not try to make thinner sheets? Hmm, I had never thought of the issue of keep a sheet thin before.

Since my daughter's brain cancer is over I can now actually work on glass. I had so many false starts prior to this year. I am excited to actually be making work. I only wish that the wonderful class I took from Avery was just a few months ago, instead of years ago. <shrug> Oh, well, onward!

KaCe


I see now. I oversimplified your question. Sorry.
'Part Sheets'...haven't heard that term. Kind of pedestrian. Needs a French touch I think.

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: adjusting sheet glass to fit my needs

Postby Morganica » Sat May 03, 2014 1:21 am

Don Burt wrote:
I see now. I oversimplified your question. Sorry.
'Part Sheets'...haven't heard that term. Kind of pedestrian. Needs a French touch I think.

Sheeetz du partay?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Don Burt
Posts: 537
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: adjusting sheet glass to fit my needs

Postby Don Burt » Sat May 03, 2014 12:42 pm

There you have it. That's a proper technique name. I'll use it. I plan to be an Emerging Artist one day.

Joyce Walters
Posts: 80
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: adjusting sheet glass to fit my needs

Postby Joyce Walters » Sat May 03, 2014 1:26 pm

Your repartee makes me smile...
Joyce

KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: adjusting sheet glass to fit my needs

Postby KaCe » Sat May 03, 2014 7:11 pm

Thank you for the replies. Do people put down thin fire and then sprinkle on the frit while on a work table? In the kiln? Is it important to keep it steady and work in the kiln on thin fire? What about any small amounts of powder that may stray if working in a kiln? Just trying to understand the best practices aspect of this technique.

I'd hate to have powder in my kiln and do damage then be told that one does it out side the kiln; or visa versa. Thank you for the help and the reply, Don. I, too, hope to emerge one day at the end of this journey and be an artist.

KaCe

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: adjusting sheet glass to fit my needs

Postby Morganica » Sat May 03, 2014 11:15 pm

I think I responded with this in the blogpost, but...We just set the sheet up on cups (so that it's easier to lift by the edges), on top of a sheet of newspaper on the worktable. If you want to save the frit, use a stack of newsprint, then after every application, lift off the work, roll up the sheet and slide the frit back into the jar. Then replace the cups/glass sheet on a fresh piece of newsprint, and do it again.

Typically, though, I don't go to that much trouble.

I don't like sifting frit on in the kiln, on thinfire or anything else, unless I'm only working in the center of the piece. If you sift in place and get beyond the sheet, it'll stick to the edges and often make sharp points that must be knocked off. Not a huge problem if you're cutting it up, but it's still a nuisance.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: adjusting sheet glass to fit my needs

Postby Valerie Adams » Sun May 04, 2014 12:10 am

Working outside your kiln, you could set up an uncoated silk screen frame and 'squeegee' on layers of colors until your desired color is achieved.

Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: adjusting sheet glass to fit my needs

Postby Terry Ow-Wing » Sun May 04, 2014 1:34 am

Valerie Adams wrote:Working outside your kiln, you could set up an uncoated silk screen frame and 'squeegee' on layers of colors until your desired color is achieved.




Where do you buy your uncoated screens - :?: someone gave me a name of a company but they only do wholesale - I would not be buying enough to establish a wholesale purchase of screens. Someone told me 130 mesh is what I should be looking for.
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: adjusting sheet glass to fit my needs

Postby Valerie Adams » Sun May 04, 2014 2:39 pm

Terry, I buy from a wholesale supplier. But you can get 18x20 screens at places like Michael's that will work fairly well. Or, check with a t-shirt screen printer in the city, and ask if they have any; they'll usually sell a single.

Don Burt
Posts: 537
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: adjusting sheet glass to fit my needs

Postby Don Burt » Sun May 04, 2014 2:55 pm

Dick Blick on Market St. should have speedball prestretched frames and fabric by the yard.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 37 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com