Hi guys what happened to this ?? using COE96 spectrum and bullseye glass (bullseye Tekta as the base for the stringers)the full fuse program was as follow
480 per hour to 932 hold 20 minutes
asap to 1490 hold 60 mins
asap to 906 hold 60 mins
150 per hour to 200
had no problems with the fusing the blank lay around the studio for a few days
but when i stumped the piece as follows
572 per hour to 932 hold 20 mins
asap to 1202 hold 20 mins
asap to 899 hold 60 mins
212 per hour to 698
626 per hour to 176
the blank is 6 mm thick
i took the plate out at room temp ,,put it on a table top and bang!!! ,,blew up ,,it was quite cool to touch
ummm ,,,what happened??
Moderator: Tony Smith
-
- Posts: 49
- Joined: Mon Apr 01, 2013 10:02 pm
- Location: Christchurch New Zealand
Re: ummm ,,,what happened??
You cant fuse Bullseye Glass (COE 90) and Spectrum Glass (COE 96) into the same piece. They are not compatible. They will do this every time. Use Bullseye only with Bullseye, and Spectrum only with Spectrum.
Re: ummm ,,,what happened??
and slow your schedules down!
Re: ummm ,,,what happened??
Yea, that schedule is extremely weird. Such precise numbers, for what reason? 572 per hour? 626 per hour? 212 per hour to 698?
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: ummm ,,,what happened??
The temps are nice, even centigrade numbers converted to Fahrenheit, which become really strange numbers.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Re: ummm ,,,what happened??
Nice look you had going on there with the stringer. Would loved to have seen your face when it let go. If you keep pushing the boundaries with your work you'll get similar days. This site is where you'll build a strong foundation to work from. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!