I'm looking in the Bullseye Catalog (9), and notice that Dense White isn't listed. I know it was discontinued a while back, but I also thought they began production at some point again. I have 2 full sheets, and someone who wants to buy them. Don't even know what to ask for them, should I get rid of them. And no, I'm not organized enough to know what I paid for them, or even when I got it. :0(( trying to figure out a fair price.
lbailey
Posts: 86
Joined: Fri Oct 26, 2012 2:53 pm
Location: FL Panhandle

Re: Dense white

Post by lbailey »

I'd hang on to them if I were you, I believe this is the white that is used with French Vanilla for some pretty unique results........

(Or sell and ship to me.......)
Risa
Posts: 34
Joined: Tue Jul 05, 2011 12:41 pm

Re: Dense white

Post by Risa »

Just ordered some from Delphi. So it appears that it may still be in production. I'll know for sure next week when it arrives and I test it.