paper between two sheets of glass

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
raphy
Posts: 27
Joined: Sun Jul 02, 2006 8:22 pm
Location: los angeles

paper between two sheets of glass

Post by raphy »

Sounds silly but can I put a picture inbetween two pieces of glass. Would it burn out? or worse cause a fire?
Thank you. Raphy
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: paper between two sheets of glass

Post by Bert Weiss »

To burn it needs oxygen. Without oxygen it will become charcoal. With oxygen it will become fire.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: paper between two sheets of glass

Post by Morganica »

The organics will usually burn out in the kiln and may or may not leave a bit of ash behind--most layups aren't airtight and at burnout temps (600-700F) the glass hasn't yet softened and sealed in/out air. The real question is, though, what else the paper leaves behind. Some inks can stain the glass or leave a residue, and some types of paper have clay or other coatings that can also leave residue.

Also depends on how much you're using. A postage stamp-sized piece of blank cheap newsprint probably won't do much. A big piece of glossy cardstock with a photograph and text printed on both sides might. Some of the inks might stain the glass and cause a visible reaction; others won't, so you might or might not get a nice result.

If it causes a fire, it's in a kiln, which is a pretty fireproof place. I wouldn't worry unless you're burning something like the Sunday New York Times and the flames start to lick out of the vents. There is a chance that combustion could be fast enough to jolt the glass and cause it to shift position but again, you'd need a bunch of paper relative to the amount of glass.

If you're trying to fuse a photograph into glass and have it look like a photograph, search this site for "screen printing," "photo transfers," and "print-making." You'll find a fair amount of information on how to get images into glass. The folks who own this site have written a book about these techniques that's worth a look.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: paper between two sheets of glass

Post by Bert Weiss »

I have to laugh, Cynthia. Many years ago, my girlfriend was a novice jeweler. She decided to make a silver casting of a tiny plastic moose. She used the lost, little plastic moose method, of casting. She invested it with sprues and stuck it in the kiln. A fire ensued that almost killed the elements in the kiln. I have had and loved the silver moose for 30 some years. That was the last time she employed the technique...
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
AndyT
Posts: 168
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: paper between two sheets of glass

Post by AndyT »

I've taken a piece of BE thin fire did a small drawing with pencil and placed it between a base of black and clear top and it turned out fine.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: paper between two sheets of glass

Post by Morganica »

AndyT wrote:I've taken a piece of BE thin fire did a small drawing with pencil and placed it between a base of black and clear top and it turned out fine.
...and then there's leaving a layer of graphite between the glass... ;-)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: paper between two sheets of glass

Post by Peter Angel »

You could try putting kiln paper (eg bullseye thinfire) between 2 sheets of glass and fuse all that together.

I have no idea what might happen.

Pete
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
GlassCat
Posts: 24
Joined: Thu May 06, 2010 5:46 pm

Re: paper between two sheets of glass

Post by GlassCat »

Glass line sells a line of colored papers that are ment to be fired between sheets of glass. Guess what it's made of?? Thin fire!!!