Scratch on final product

Post by Deb »

After coming home from a show, I noticed a small scratch on top of my item. Normally, I would put it back in the kiln and polish it but I have glued cabochons on the bottom with E6000. Any suggestion on how to fix the scratch or how to loosen up E6000 between 2 pieces of glass? Thanks.
Deb
Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: Scratch on final product

Post by Georgia Novak »

soak it in Acetone until loose. Pour the Acetone in a container that you can put a lid on or it will evaporate before it separates the pieces.