melted glass on stainless former
Moderator: Brad Walker
-
- Posts: 41
- Joined: Sun Mar 30, 2003 11:56 am
- Contact:
melted glass on stainless former
I had a meltdown in the kiln, and have melted glass embedded on a stainless steel former. I tried to get it off by putting in a kiln to 900 degrees, then dropping it into water - a lot of the glass came off, but some remains. I do not want to sandblast it in my booth, as my grit is very fine and I don't want to contaminate it. I was wondering about other techniques to get it off, or also to spray a resist onto it, or kiln wash, and hope that the minor amount of glass still stuck to the surface will not be a problem, as i am just folding vases , not melting glass onto them.
-
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: melted glass on stainless former
Do you have diamond hand pads? You may be able to sand it off that way.
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: melted glass on stainless former
Go to a wholesale restaurant supply and ask for a martini shaker. They cost a small fraction of a floral former from a glass supplier. I bought one from each and they were identical.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
- Posts: 41
- Joined: Sun Mar 30, 2003 11:56 am
- Contact:
Re: melted glass on stainless former
I also had a ceramic stand that the stainless steel former sat on that got covered with glass. It let the glass slide onto the former, and make the ends of the vase turn a bit. It was 5.5" wide at the base, and was like a gentle slope at the end of the former. Do you have any idea where to get something like this?
-
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: melted glass on stainless former
i would dremmel it off. r.
artist, owner of wanchese art studio, marine finisher
Re: melted glass on stainless former
[quote="jerry keller"]I had a meltdown in the kiln, and have melted glass embedded on a stainless steel former. I tried to get it off by putting in a kiln to 900 degrees, then dropping it into water - a lot of the glass came off, but some remains. I do not want to sandblast it in my booth, as my grit is very fine and I don't want to contaminate it. I was wondering about other techniques to get it off, or also to spray a resist onto it, or kiln wash, and hope that the minor amount of glass still stuck to the surface will not be a problem, as i am just folding vases , not melting glass onto them.[/quote]
you can sand blast it. it won't contaminate the grit.
you can sand blast it. it won't contaminate the grit.
-
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: melted glass on stainless former
Not sure what kind of former.....but if it is one of ours i would just line it with your 1/8" paper and use it. The paper will seperate it from your next work.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com