Risa
Posts: 34
Joined: Tue Jul 05, 2011 12:41 pm

Bullseye 1015 - reacts with silver

Postby Risa » Thu Nov 13, 2014 5:40 pm

This glass is supposed to react with silver foil and result in a gold finished look.
Has anyone tried this yet? I bought a piece and don't know what to do with it, so I'd love to see other projects.

Kim Manley
Posts: 17
Joined: Thu Feb 09, 2012 10:00 am

Re: Bullseye 1015 - reacts with silver

Postby Kim Manley » Fri Nov 14, 2014 7:47 am

I've seen a box by Nathan Sandberg made with this glass. He brought it to Aus. In October. I don't have a photo but there is clearly a reaction. Bullseye won't ship any to Australia yet so haven't tried it.

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Bullseye 1015 - reacts with silver

Postby Valerie Adams » Fri Nov 14, 2014 9:04 pm

There was an artist showing photos of her testing that glass on the FB group called Fused Glass Fanatics.
You can join the group and search for 1015; it'll bring up her photos.

Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: Bullseye 1015 - reacts with silver

Postby Andrea R » Sat Nov 15, 2014 1:15 pm

Is 1015 new?
Image
"C'est Moi (Its Me)"

Brad Walker
Site Admin
Posts: 1349
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Bullseye 1015 - reacts with silver

Postby Brad Walker » Sat Nov 15, 2014 2:18 pm

Andrea R wrote:Is 1015 new?


1015 is Reactive Silver Clear. Special production at the present time, but may be in their line down the road.

Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: Bullseye 1015 - reacts with silver

Postby Andrea R » Sat Nov 15, 2014 2:30 pm

Brad Walker wrote:
Andrea R wrote:Is 1015 new?


1015 is Reactive Silver Clear. Special production at the present time, but may be in their line down the road.


Thanks Brad think I will need to get some of that!!!

a
Image
"C'est Moi (Its Me)"


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 46 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com