I remembered from something that I cover a circle with pebbles then tac and slump. I have one layer circle and covered it with pebbles. Need suggestions for firing schedule - I don't want to loose the texture but I want the pebbles to most definately be attached. Thanks
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Tac fuse for pebbles

Post by rosanna gusler »

wont work. glass will break on cool dowd. r.
artist, owner of wanchese art studio, marine finisher
Charlotte Kay
Posts: 15
Joined: Sat Dec 12, 2009 10:43 pm
Location: Northern California

Re: Tac fuse for pebbles

Post by Charlotte Kay »

I think she means fused glass "pebbles" that you make from breaking up a pattern bar or pot melt. Kinda like frit balls.

I have used either the 2-layer or the 3-layer fusing schedules for a tack fuse on fusedglass.org Depends on how thick your base circle is and how thick your pebbles are. You want to use the thickest measurement in your calculations.
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Tac fuse for pebbles

Post by Valerie Adams »