Sharpie paint pens - WarmGlass.com

Sharpie paint pens

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
vblue
Posts: 98
Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas

Sharpie paint pens

Postby vblue » Wed Dec 17, 2014 12:11 am

Has anyone successfully used the Sharpie paint pens in the kiln? (not the permanent marker type.)

Thanks,
Vernelle

Aglassygirl303
Posts: 47
Joined: Sun Nov 08, 2009 10:08 pm

Re: Sharpie paint pens

Postby Aglassygirl303 » Wed Dec 17, 2014 1:11 am

Yes. I love them. The Oil Based ones. I made 35 Red Cardinals and offered people personal names on them. They came out beautifully. I used the extra fine point

Georgia Novak
Posts: 28
Joined: Wed Jun 04, 2003 2:54 am

Re: Sharpie paint pens

Postby Georgia Novak » Wed Dec 17, 2014 3:20 pm

How high did you fire the paint from the pens?

vblue
Posts: 98
Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas

Re: Sharpie paint pens

Postby vblue » Wed Dec 17, 2014 11:15 pm

I tried the silver and gold pens. The gold turned dark but the silver was okay. I took it to around 1500. Have you tried any other colors?

Aglassygirl303
Posts: 47
Joined: Sun Nov 08, 2009 10:08 pm

Re: Sharpie paint pens

Postby Aglassygirl303 » Fri Dec 19, 2014 1:19 pm

I used the gold after I fired the piece

Aglassygirl303
Posts: 47
Joined: Sun Nov 08, 2009 10:08 pm

Re: Sharpie paint pens

Postby Aglassygirl303 » Fri Dec 19, 2014 1:19 pm

I used the gold after I fired the piece


Post Reply

Return to “Techniques and Tools”

Who is online