hi there one and all.. these bottles have a lot of sentimental value, so i only get one try at slumping them ,,,i want to try and dam two sides as they slump,,,has anyone tried this and have success?? any input would be appreciated..and yes i would use some thin fire or kiln wash on the dams
many thanks as always,,, paul
Attachments
DSCN2178.JPG
DSCN2177.JPG

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: sentimenal bottles

Postby rosanna gusler » Fri Feb 20, 2015 7:06 pm

why dam?
artist, owner of wanchese art studio, marine finisher

Paul Schulz
Posts: 49
Joined: Mon Apr 01, 2013 10:02 pm
Location: Christchurch New Zealand

Re: sentimenal bottles

Postby Paul Schulz » Fri Feb 20, 2015 7:18 pm

i want to make a pair of matching plates using the shape of the bottles ,so when they have been slumped they can lay side by side with out a big difference in the over all shape

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: sentimenal bottles

Postby rosanna gusler » Fri Feb 20, 2015 8:52 pm

so you are going to lay them on their side with a dam on the flat side? it could work but you will get some 'interesting' folds i think............ i would do a test run with 2 regular clear bottles set up just like that. you will have to put a couple of little pieces of balled up fiber under the edges of the bottles opposite the dams to keep them from rolling. fire the test bottles and then you will be able to get a fairly good idea about how your special bottles will behave....... pay close attention to how thick the glass is where itfolds over and figure your anneal accordingly. if you want i can go out and look up a bottle schedule . too fast and you can trap some pretty mongo bubbles. good luck. r.
artist, owner of wanchese art studio, marine finisher

Paul Schulz
Posts: 49
Joined: Mon Apr 01, 2013 10:02 pm
Location: Christchurch New Zealand

Re: sentimenal bottles

Postby Paul Schulz » Sat Feb 21, 2015 3:41 am

Good idea =D> ,,,,,not sure why i didn't think of that,,, #-o am starting kiln overnight will post in 2 days

Paul Schulz
Posts: 49
Joined: Mon Apr 01, 2013 10:02 pm
Location: Christchurch New Zealand

Re: sentimenal bottles

Postby Paul Schulz » Sun Feb 22, 2015 6:21 pm

well i got the sort of finish i am hoping to get ,,,all so got some very heavy folding, 25mm thick.i think i may have to rethink my firing program and allow more time for annealing,,,Any thoughts
150 540 20
150 620 15
315 680 29
315 804 20
999 482 60
32 427 30
49 370 00
66 100 00
Attachments
DSCN2183.JPG
DSCN2181.JPG

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: sentimenal bottles

Postby rosanna gusler » Mon Feb 23, 2015 12:50 pm

i anneal bottle glass at 1000f. then drop at 85f/hour to 700f. i would anneal for at least 1.5 hours. you only have one shot at this so why skimp. r.
artist, owner of wanchese art studio, marine finisher


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: Google [Bot] and 6 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com