need a thin black line - WarmGlass.com

need a thin black line

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

need a thin black line

Postby Andrea R » Sat Mar 28, 2015 9:51 pm

Making an out line and need the line thin have Josephine glass black and Josehine outline black.
Will tack fuse and then cap and fire to full 1475 or around there do you think the Josephine will hold up or burn out?
I also have Paradise.
What will work best??
As aways thanks for the help dont know what I would do with out you guys :-)

Andrea
Image
"C'est Moi (Its Me)"

Don Burt
Posts: 536
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: need a thin black line

Postby Don Burt » Sat Mar 28, 2015 11:04 pm

The Josephine glass black has a low melting frit in it. It would dissipate the most of the three. I guess that either of the other two will do as well as anything else available. Rather than putting stock in my guess you could of course test them.

Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: need a thin black line

Postby Andrea R » Sat Mar 28, 2015 11:28 pm

Don Burt wrote:The Josephine glass black has a low melting frit in it. It would dissipate the most of the three. I guess that either of the other two will do as well as anything else available. Rather than putting stock in my guess you could of course test them.

I new I should test them ...........but Easter is so close!!
Don I just love you!!You alwat get back fast and with great advice.
Thanks
a
Image
"C'est Moi (Its Me)"

Kevin Midgley
Posts: 698
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: need a thin black line

Postby Kevin Midgley » Sun Mar 29, 2015 2:07 am

bent black stringer?

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: need a thin black line

Postby Valerie Adams » Tue Mar 31, 2015 5:03 pm

I love the new .5 mm stringers from Bullseye for thin lines.

I also use Reusche enamels with clove oil, and have fired the high-fire formulas to 1500°. My tests with Paradise Paints (I have several jars of the mixed paint) show they hold up to at least 1440°.

Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: need a thin black line

Postby Andrea R » Tue Mar 31, 2015 9:20 pm

Valerie Adams wrote:I love the new .5 mm stringers from Bullseye for thin lines.

I also use Reusche enamels with clove oil, and have fired the high-fire formulas to 1500°. My tests with Paradise Paints (I have several jars of the mixed paint) show they hold up to at least 1440°.

I agree the BE thin stringers are great but I need enamel I also use clove oil I love the smell the houes has for days:) Just me.
I did a test and capped it was fine up to a full fuse so testing testing always pays!!
thanks A
Image
"C'est Moi (Its Me)"


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com