It is my first slump firing. Do I place the mold directly on the shelf, or should i put it on stilts to aid in air circulation? It has four small holes in the bottom, but wonder how well the air circulates if it is sitting on a shelf. thanks.

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Place slump mold directly on kiln Shelf?

Postby rosanna gusler » Wed Apr 08, 2015 10:18 am

i like to elevate my molds off the shelf. it helps to avoid heat shocking the shalf and aids in evenivity. you can also put molds on the floor of the kiln if height is an issue.r.
artist, owner of wanchese art studio, marine finisher

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Place slump mold directly on kiln Shelf?

Postby Bert Weiss » Wed Apr 08, 2015 2:14 pm

For a slump firing, all a shelf is doing for you is adding mass to the kiln load. This costs money to heat up and takes more time to cool down. Nothing is gained at all. It is a good idea to raise your slump mold off of the floor with 3 points of contact, then you should level it. The most important factor is to make sure the holes in the mold have a place where air can actually escape. leaving a slump mold on the floor may not be ideal, but it will work fine as long as the holes are cleared. There are a lot worse things you can do. I rarely use shelves for anything. Mostly I fuse directly on my kiln floor, which is covered with fiber blanket,and/or a sand casting mold.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

conboc
Posts: 11
Joined: Wed Apr 08, 2015 12:17 am

Re: Place slump mold directly on kiln Shelf?

Postby conboc » Wed Apr 08, 2015 3:59 pm

Thank you so much for writing in! Appreciate your help.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 7 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com