finding a diamond grinding wheel
Moderators: Brad Walker, Tony Smith
finding a diamond grinding wheel
HI. I need to find a supply of 4" concave diamond wheel, sometimes called cup wheel for my angle grinder. Also, asking Bob at HIS. I have used at Pilchuck, but all I find are straight profiles. I checked Ebay, granite stores, and online and am having trouble. Anyone know? If not, I will be at Pilchuck next month and can try and find out.
-
- Site Admin
- Posts: 1489
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: finding a diamond grinding wheel
How wide? What grit?
I have some on hand, might have something you can use.
I have some on hand, might have something you can use.
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: finding a diamond grinding wheel
Hi Dick,
Have you looked at Abrasive Technology?
https://store.abrasive-tech.com/Catalog ... talogID=48
Tony
Have you looked at Abrasive Technology?
https://store.abrasive-tech.com/Catalog ... talogID=48
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Re: finding a diamond grinding wheel
Thanks Tony and Brad. Looking for 4" with 5/8" x 11 threads for angle grinder. Coarse or rough grit. The photos show the idea of the wheel, as I have seen several shapes, but basically like this. My new work uses this as in the other photo.
-
- Site Admin
- Posts: 1489
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: finding a diamond grinding wheel
Don't have that one, Dick, but I'll check my supplier to see if they make something similar.
-
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: finding a diamond grinding wheel
Inland diamond?