Pre-firing Stringers
Moderator: Tony Smith
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Pre-firing Stringers
Hello ! I wonder which simple quick schedule I can use to pre-fire Stringers to avoid rolling ? Jan de Jong
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Pre-firing Stringers
This is one method that does not need firing before use.
http://glasstips.blogspot.co.uk/2015/07 ... ngers.html
http://glasstips.blogspot.co.uk/2015/07 ... ngers.html
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Pre-firing Stringers
@ Steven Richard: Thank you for your answer, but is there a simple, quick firing-schedule known for this stringers ?? I have to do much stringers, so my choice is pre-firing. greetings from Holland, Jan
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Pre-firing Stringers
I guess you'd have to test for your kiln, but when I slump stringer, I fire afap to 1250° and hold until visually confirmed. If you're trying for a flat side, you'd probably have to fire a little hotter.
I'd choose a temp to start with and monitor them. When they should be done, quickly remove one with a long needle nosed plier (and gloves!), and check it. Add time as necessary.
I'd choose a temp to start with and monitor them. When they should be done, quickly remove one with a long needle nosed plier (and gloves!), and check it. Add time as necessary.
Re: Pre-firing Stringers
Liquid Stringer Medium advertisement makes this claim, 'Its primary benefit is that it will withstand elevated temperatures thus holding the glass particles in place until they are sticky enough to bond together on their own.' This seems to indicate that you can use this product to tack the stringers in place and fire while the Liquid Stringer Medium holds the the stringers in place.
I have used the product for other purposes and find that it does burn off clean.
I have used the product for other purposes and find that it does burn off clean.
Jerry
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Pre-firing Stringers
OK. As fast as possible to 740C, off
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Pre-firing Stringers
Okay.....thank you all for your respons ! greetings from Holland, Jan de Jong