Borax or boric acid?
Which is a stronger flux, borax or boric acid? Are there any other notable differences in the way they work between the two?
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Borax or boric acid?
All I know is that 20 mule team borax works. I never tried anything else. Some will crystalize at the bottom of the bottle, just pour the liquid off and it works. This stuff is cheap.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Borax or boric acid?
borax: Na2B4O7
boric acid: H3BO3
they are not interchangeable and not the same.
boric acid: H3BO3
they are not interchangeable and not the same.