After slumping a large piece of glass - 23"x23", I did not like the configuration, so put it back into the kiln for a re-slump. The results were better, but I found a small chip near the top edge where the floral former held the glass to rest upon.
Is re-slumping a problem with this sort of result?
chip in edge of floral formed vase
Moderator: Brad Walker
-
- Posts: 41
- Joined: Sun Mar 30, 2003 11:56 am
- Contact:
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: chip in edge of floral formed vase
I'll guess this was caused by the glass sticking to the mold. This could interfere with a good anneal.