Here is a stupid question. The first segment is 300 per hour to 1350, then segment 2 is Afap to 960. What temp do I set the kiln at to go afap to 960.
Thanks
What temp is afap
Moderators: Brad Walker, Tony Smith
-
- Site Admin
- Posts: 1489
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: What temp is afap
For most controllers, it's 9999, which is as fast as can be programmed.