I have been sawing patternbars on my 10" wetsaw with a Husqvarna Diamond glass blade. Lately the bars 3\8x3\8. Are breaking quite a bit. Have water streams directed to the cut, there is not excessive vibration, blade is dressed frequently. Is it time for a new blade? How do you tell? The bars were well annealed 900 for 2 you then 25 per/hr to 800 75 to 700 then off.Thanks
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
- Posts: 308
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Diamond Blade
Have you dressed the blade recently?
Jim
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
-
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Diamond Blade
Are you using a blade stabilizer? That made a big difference on my 10" saw.
-
- Posts: 254
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Diamond Blade
dress it frequently with a stone from HIS, no stabilizers might try that..read somewhere you can use old 7" blades as stabilizers?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Diamond Blade
Stabilizer. Definitely helps.
HIS glassworks.
The other Jim
HIS glassworks.