Is there a way to clean off the accumulated kiln wash on ceramic molds. Every time I slump pieces of kiln wash get embedded on my piece.

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: ceramic molds

Postby Brad Walker » Mon Feb 13, 2017 2:21 pm

User wet/dry sandpaper, fine.

When you reapply, you don't need that many coats. Two or three will work fine.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: ceramic molds

Postby Kevin Midgley » Mon Feb 13, 2017 3:04 pm

drywall sanding mesh

Sharol
Posts: 118
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: ceramic molds

Postby Sharol » Mon Feb 13, 2017 3:21 pm

Yes, drywall sanding mesh works best. It's also what I use to clean my shelves. Works great. Wear gloves though. It's rough on your hands.

seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: ceramic molds

Postby seachange » Mon Feb 13, 2017 9:37 pm

Hi

To clean shelves: I place them on a couple of pages of newspaper. Spray the surface with water to keep the dust down, scrape with a paint scraper. It forms small flakes that are collected into the newspaper. If needed I wash any left over rests under a tap (outside).

To clean molds: I wash them with a plastic scrubby in a bucket of water. Rinse and leave to dry, then reapply separator.

Please consider I am doing this outside. Wouldn't be good for the plumbing.

Best regards, seachange

BobbieMatus
Posts: 50
Joined: Tue Jul 08, 2003 12:21 am

Re: ceramic molds

Postby BobbieMatus » Tue Feb 14, 2017 12:40 pm

thanks everyone

JestersBaubles
Posts: 696
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: ceramic molds

Postby JestersBaubles » Wed Feb 15, 2017 3:33 pm

If kiln wash gets embedded in your glass during a slump, then I think you are slumping at too high of a temperature.

2 cents,
Dana W.

DonMcClennen
Posts: 370
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: ceramic molds

Postby DonMcClennen » Wed Feb 15, 2017 5:45 pm

I coated my moulds once when they were new and never again!... some I've been using 20yrs. never had to recoat. I agree with the last post your top slumping temp should be low enough that melting against mold should not be happening!!
"The Glassman"


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 68 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com