latest and first in an investigation of frit and pattern. This one has 3 colors, one is reactive... I combed the lines in the frit and stenciled the lighter shapes. These are 10" square and were for a show at the National Corvette Museum. They were inspired by the older Vette's. They should be hung on the wall with cleats, not meant to live on these display brackets.
Latest Piece
Moderator: Brad Walker
-
- Posts: 80
- Joined: Thu Nov 08, 2007 12:06 am
- Location: Stevensville MT
Re: Latest Piece
Thank you for sharing!
I really like the color work. Strong lines, strong contrast.
I won't forget the precision of your combing frit, and hope to use that someday soon.
Joyce
I really like the color work. Strong lines, strong contrast.
I won't forget the precision of your combing frit, and hope to use that someday soon.
Joyce
Re: Latest Piece
Thanks, the combing can be a challenge. This was with a thin bamboo skewer. The red is from the first firing and an additional layer of red frit. It is not as intense as it is in the photo.