Kiln is rewired, experiments starting.
I've noticed that after sandblasting, the glass is susceptible to staining, from lots of things, some of it seems permanent even without firing.
Thinking of trying copper sulphate, that puts greenish tinge on bronze castings, or rust in a solvent of some type. Using float.
Any clues, references welcome. As usual I'm happy to share anything I find out.
Thanks. Peter.
metalic stains after blasting
Moderators: Brad Walker, Tony Smith
-
peter cummings
- Posts: 71
- Joined: Mon Jan 19, 2004 4:05 am
- Location: sale,s.e.vic,australia
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: metalic stains after blasting
Alex Bernstein fuses steel to the surfaces of his cast glass: http://alexbernsteinglass.com/artwork/ He makes some really fascinating sculptures.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: metalic stains after blasting
essentially any oil based paint will stick in the pores of the blasting.
If you buff and then repeat buff and repeat, you can build up a finish.
Done often enough you have the paint forming a solid film and colour.
If you buff and then repeat buff and repeat, you can build up a finish.
Done often enough you have the paint forming a solid film and colour.
-
peter cummings
- Posts: 71
- Joined: Mon Jan 19, 2004 4:05 am
- Location: sale,s.e.vic,australia
- Contact:
Re: metalic stains after blasting
Thanks Brad and Kevin. That is some studio Alex has, and looks interesting works. I can't get right into the pictures though, either website or flickr problem. I'll try the paint as Kevin suggested, maybe like my recent wood stain effort, painters oil paint mixed with gum turps, apply and wipe back. It's an organic Galle look I'm after.
I'll let you know, and it's good to catch up again.
I'll let you know, and it's good to catch up again.
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: metalic stains after blasting
Peter,
Check out Sculpt Nouveau. http://www.sculptnouveau.com
They have a YouTube page as well.
They have patinas and base finishes for all materials that replicate many different oxides.
Tony
Check out Sculpt Nouveau. http://www.sculptnouveau.com
They have a YouTube page as well.
They have patinas and base finishes for all materials that replicate many different oxides.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
peter cummings
- Posts: 71
- Joined: Mon Jan 19, 2004 4:05 am
- Location: sale,s.e.vic,australia
- Contact:
Re: metalic stains after blasting
Thanks Tony. Beautiful colours and finishes. I see they "road freight" and I've sent email questions. I'll also look for metal finishes over here.
-
peter cummings
- Posts: 71
- Joined: Mon Jan 19, 2004 4:05 am
- Location: sale,s.e.vic,australia
- Contact:
Re: metalic stains after blasting
Yah Tony. Sculptnouveau have a distributor in Australia, that has opened a new store in Melbourne. My capital. They tell me some of their products will work on glass. A trip to town coming up.
Peter.
Peter.