The right torch for bullseye rods

Post here with questions and topics relating to making glass jewelry.

Moderators: Tony Smith, Brad Walker

Post Reply
Maggie Abdel Rahman
Posts: 36
Joined: Tue Nov 06, 2007 10:16 am

The right torch for bullseye rods

Postby Maggie Abdel Rahman » Mon May 29, 2017 4:55 pm

I tried to make little leaves using bullseye rods. I used a dual-fuel torch (oxygen and propane), but the glass colors changed and the clear glass rod turned greyish. Is a single fuel torch better with soft glass ?

Tom Fuhrman
Posts: 176
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: The right torch for bullseye rods

Postby Tom Fuhrman » Fri Jun 02, 2017 10:49 am

Dual is required, but it must be surface mix, not premix. I've been using a Nortel minor for many years and now have switched to a Bethlehem Alpha, You also have to have your flame adjusted correctly and work way out in the end of the flame.

Maggie Abdel Rahman
Posts: 36
Joined: Tue Nov 06, 2007 10:16 am

Re: The right torch for bullseye rods

Postby Maggie Abdel Rahman » Sat Jun 03, 2017 10:24 am

Many thanks Tom

jim simmons
Posts: 441
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: The right torch for bullseye rods

Postby jim simmons » Sat Jun 03, 2017 8:44 pm

Main thing is to use the proper gas mix, and work way out in the flame.

Maggie Abdel Rahman
Posts: 36
Joined: Tue Nov 06, 2007 10:16 am

Re: The right torch for bullseye rods

Postby Maggie Abdel Rahman » Sun Jun 04, 2017 1:44 pm

Thank you for your tip Jim


Post Reply

Return to “Jewelry Making”

Who is online

Users browsing this forum: No registered users and 1 guest

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron