Removing kiln wash to apply Boron Nitride

Postby StephenieWooten » Sun Jul 02, 2017 9:32 am

Hello. I recently acquired some molds that were coated in kiln wash. I would like to know if I can remove this wash and apply Boron nitride. And if so what would be the easiest way to remove it? Good ole scrubbing?
Thanks for any suggestions and help.

DonMcClennen
Posts: 345
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Removing kiln wash to apply Boron Nitride

Postby DonMcClennen » Sun Jul 02, 2017 10:46 am

The grid like sandpaper used by drywallers will make short work of removing kilnwash.
"The Glassman"


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 4 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron