Will a nice layer of whiting spread on the shelf with a texture pattern pressed into the surface serve as a mold for kilncarving? Or is it too soft? Can it be stiffened?
Jin "The Hobbyist"
Whiting as texture mold
Moderator: Brad Walker
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Whiting as texture mold
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Whiting as texture mold
I have mixed whiting with water to a thick cream consistency and applied it to coated kilnshelf with a cake decorating icing sqeezebag to form tree images. Sets to a hard enough image to set 1/4" glass on top. (coat with kilnwash before placing glass on top) You should probably experiment!