Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Mon Apr 16, 2018 11:30 am

Hello . I have not posted in awhile and have missed you all so thought I would catch up on what I have been up to. Casting large color bars and then slicing them up to take to the hot shop. Just simply exciting and has allowed me to do things that I could not do before. Working in Bullseye Glass does not stop me from going to the hot shop and Ryan Bavin is truly an inspiration and just knows how to make my ideas and bars into round forms that is a bit more difficult for us all.
IMG_8350.JPG
VAALR_010.jpg

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Mon Apr 16, 2018 11:34 am

VAALR_035.jpg
VAALR_004.jpg

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Mon Apr 16, 2018 1:12 pm

php7epM5dAM.jpg
php7epM5dAM.jpg (51.57 KiB) Viewed 7180 times
Attachments
php8UaO3DAM.jpg
php8UaO3DAM.jpg (22.68 KiB) Viewed 7180 times
phpMkqarJAM.jpg
phpMkqarJAM.jpg (61.6 KiB) Viewed 7180 times
Last edited by twin vision glass on Mon Apr 16, 2018 1:19 pm, edited 1 time in total.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Mon Apr 16, 2018 1:13 pm

phpATf3rPAM.jpg
A piece that is being put back in the kiln to then fuse again and get ready to take to hot shop
phpATf3rPAM.jpg (42.14 KiB) Viewed 7180 times
phpKlCEMnAM.jpg
phpKlCEMnAM.jpg (45.58 KiB) Viewed 7179 times
phpSkH4r2AM.jpg
phpSkH4r2AM.jpg (50.1 KiB) Viewed 7179 times

Kevin Midgley
Posts: 694
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Getting ready to blow out Color Bar in HOT shop

Postby Kevin Midgley » Tue Apr 17, 2018 12:25 am

impressive work being created.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Tue Apr 17, 2018 9:25 am

Hi Kevin. Hope you are well . I love it back in the hot shop again.

Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Getting ready to blow out Color Bar in HOT shop

Postby Warren Weiss » Tue Apr 17, 2018 9:49 am

Beautiful!! A new dimension.

Warren

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Tue Apr 17, 2018 11:20 am

I have really enjoyed getting back into the hot shop and Ryan Bavin just understands so well how the Bullseye Glass Blows out in large chunks and sections and how to maximize the interesting things going on inside. The important part is to remember what will actually be inside when blown out and what is on the outside when all is said and done

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Fri May 11, 2018 2:56 pm

phpZ5hzPEAM.jpg
phpZ5hzPEAM.jpg (48.35 KiB) Viewed 7012 times
phpz6SesDAM.jpg
phpz6SesDAM.jpg (47.61 KiB) Viewed 7012 times
phpIlj72gAM.jpg
phpIlj72gAM.jpg (47.52 KiB) Viewed 7012 times
Hot shop fun and happy with Vitrigraph pull on outside

Ed Cantarella
Posts: 153
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Getting ready to blow out Color Bar in HOT shop

Postby Ed Cantarella » Sat May 12, 2018 8:32 am

WOW - really gorgeous.
I would really dig manipulating glass like that, after some intense instruction. Too cool.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Sat May 12, 2018 8:47 am

Thank you Ed, I love taking the Bullseye Glass to the hot shop and manipulating it. The large cast glass bars are the best to begin with for me for a more organic look.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Mon May 21, 2018 10:49 am

phpMh3DA6AM.jpg
phpTpcyNaAM.jpg
phpTpcyNaAM.jpg (46.63 KiB) Viewed 6892 times
always fun to go get a nice pic

Sharol
Posts: 111
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Getting ready to blow out Color Bar in HOT shop

Postby Sharol » Sat Jun 16, 2018 12:22 am

It is so great to see your work posted here again! I’ve missed you! What a wonderful thing for you to once again merge these two glass methodologies. Inspirational. Thank you for posting the pictures of your adventure.
Sharol

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Getting ready to blow out Color Bar in HOT shop

Postby twin vision glass » Sat Jun 16, 2018 9:22 am

Hi Sharol, It is great to share again with everyone. I tooo have missed posting in Warm Glass.
phphS7OcoPM.jpg
My twin and I are having fun pulling out the slices on the torch as well. It is just so fun to take this beautiful material and manipulate it hot.


Post Reply

Return to “Photos and Stuff”