Wetbelt sander belts breaking - WarmGlass.com

Wetbelt sander belts breaking

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Wetbelt sander belts breaking

Postby Greg Rawls » Wed Oct 03, 2018 7:11 am

I have a bunch of belts for my wetbelt sander that are a few years old that are splitting at the seam after a few minutes of use. Consistently! Does the glue that holds the belt together have a shelf life? Anyone else had this problem?
Greg

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wetbelt sander belts breaking

Postby Brad Walker » Wed Oct 03, 2018 8:33 am

Funny you mention this, Greg. I had two split on me just a couple of weeks ago. Don't know why. The belts were purchased several years ago, so perhaps there's a shelf life issue. But I've never had the problem before.

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Wetbelt sander belts breaking

Postby Tony Smith » Thu Oct 04, 2018 7:30 am

Are these full-size belts or Covington size? I've never heard of belts coming apart, but I suppose it's possible as the glue hardens over time.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wetbelt sander belts breaking

Postby Brad Walker » Thu Oct 04, 2018 8:36 am

Tony Smith wrote:Are these full-size belts or Covington size? I've never heard of belts coming apart, but I suppose it's possible as the glue hardens over time.


Full-size. I'd never heard of it either until it happened twice this past month.

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Wetbelt sander belts breaking

Postby Marty » Thu Oct 04, 2018 9:08 am

I've never had one split either. Mine fray.
I have to change some out and the new ones are several years old. Stay tuned.

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Wetbelt sander belts breaking

Postby Greg Rawls » Fri Oct 05, 2018 7:49 am

These belts are 41-1/2 x 3. One belt breaking would not be an issue, but every time I replace the belt from my old stash (and these are maybe 4-6 years old), they work for a few minutes then split right at the seam.
Greg

FusedLightStudio
Posts: 55
Joined: Wed Jan 24, 2018 1:33 pm
Location: Georgia
Contact:

Re: Wetbelt sander belts breaking

Postby FusedLightStudio » Fri Oct 05, 2018 8:35 am

Greg Rawls wrote:These belts are 41-1/2 x 3. One belt breaking would not be an issue, but every time I replace the belt from my old stash (and these are maybe 4-6 years old), they work for a few minutes then split right at the seam.


Yep. Same exact problem. Had to buy new belts. But I cut up the old belts into small pieces to use as wet sandpaper for curves.
Lisa Schnellinger
Atlanta, GA

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Wetbelt sander belts breaking

Postby Marty » Fri Oct 05, 2018 9:54 am

Marty wrote:I've never had one split either. Mine fray.
I have to change some out and the new ones are several years old. Stay tuned.


Full sized belts, from HIS.

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Wetbelt sander belts breaking

Postby Greg Rawls » Sat Oct 06, 2018 7:33 am

FusedLightStudio wrote:
Greg Rawls wrote:These belts are 41-1/2 x 3. One belt breaking would not be an issue, but every time I replace the belt from my old stash (and these are maybe 4-6 years old), they work for a few minutes then split right at the seam.


Yep. Same exact problem. Had to buy new belts. But I cut up the old belts into small pieces to use as wet sandpaper for curves.


That is a REALLY GOOD IDEA! Thanks!
Greg

Marian
Posts: 57
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: Wetbelt sander belts breaking

Postby Marian » Mon Oct 15, 2018 2:11 am

I had that happen with a batch of belts also, from CRL. They work for 15 minutes and then let go. They were a few years old when I got around to needing them. It was only one size that broke. I bought new different ones from HIS.

ejgiebel
Posts: 11
Joined: Mon May 11, 2009 7:50 pm

Re: Wetbelt sander belts breaking

Postby ejgiebel » Wed Apr 03, 2019 1:30 pm

Bit delayed in my response, but I saw a YouTube video on this a while back. Get some seam tape (not actually tape, but the fabric material they use to strengthen clothing seams) from a fabric store. Cut the seam tape to the width of the belt, one layer thick (seems to me it's folded over on itself, so you just want one layer). Scrape off the old seam material with a razor blade. Place the ends of the belt grit side down on a piece of wax paper (so the glue won't stick to it if it seeps through the seam), firmly hold the belt in place with the seam matching. Spread a thin layer of Gorilla Glue (it's water proof, super glue is not) on the belt. You want enough to hold, but don't get wild and crazy since the Gorilla Glue expands and can push through the seam onto the grit. Place the seam tape in the glue, add a bit more glue to saturate the tape. Spread the glue flat, place a weight (again, use wax paper because Gorilla Glue really sticks) over the seam and let dry (I think 24 hours is their recommend full cure time). You can make the piece of tape slightly larger than the belt and trim it once the glue dries (but the glue will be hard).

I repaired a belt that lasted about 30 minutes when new 2 years ago (OK, don't use the belt a lot, but I've used it 10 hours since then) and it is still holding strong.

Ed


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 44 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron