I have a couple unopened samples of Zircar's Mold Mix 6, and they are almost rock solid. Has anyone tried to reconstitute this material with a little water and perhaps a blender? According to Zircar, it might not be worth the effort. I want to paint some on a mold made from Zircar sheet material, for a better texture and finish. Thanks.
Nikki

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Mold Mix 6

Postby twin vision glass » Sun Aug 04, 2019 9:33 pm

I think I am sad to say that it would not be good . So sorry to break the bad news. It is SOOO wonderful when it is new and like thick cream

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Mold Mix 6

Postby twin vision glass » Sun Aug 04, 2019 9:34 pm


Nikki ONeill
Posts: 165
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Re: Mold Mix 6

Postby Nikki ONeill » Mon Aug 05, 2019 9:01 am

Thank You Leslie for the wonderfully presented video. Clear, excellent instructions. I want to mention that I took my rock solid sample and immersed it in water for a day and it became workable. Mixing with a hand mixer made it creamy again. I hope the fibers are still in good shape!

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Mold Mix 6

Postby twin vision glass » Mon Aug 05, 2019 9:32 am

Well that is great. Let us know how it works for you. Try a small cast piece first perhaps open face . Les

Nikki ONeill
Posts: 165
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Re: Mold Mix 6

Postby Nikki ONeill » Mon Aug 05, 2019 10:16 am

Good idea. thanks Leslie!


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: Google [Bot] and 6 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com