Those of you in the know, does this System 96 glass color strike? If this is the orange I think it is, it color shifts to orange/ brown at fusing temps.

#96-675.5G Godiva

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Does this Color Strike?

Postby Judd » Wed Sep 25, 2019 10:00 am

The pic didn't attach. Sorry.

Nor did it again. Well, the color is easily Google-able. So sorry.

Brad Walker
Site Admin
Posts: 1394
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Does this Color Strike?

Postby Brad Walker » Wed Sep 25, 2019 10:53 am

Probably strikes, most oranges/reds do.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 23 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com