enamel suggestions

Post by peter cummings »

Enamel suggestions please for a thin, watercolour wash look, probably airbrushed on. Float maybe. I'm in Australia which might limit it. I don't think sifted powders will give me a smooth wash look. Oh and can I fire it enamel down for a smooth clear top? Thanks folks.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: enamel suggestions

Post by Kevin Midgley »

Multiple firings, multiple coats will possibly give you the result you want.
Silver stains fire down onto disposable whiting. (you don't want random silver in your kiln)
Paints/enamels are fired face up unless you don't mind them sticking to whatever they are place on to fire.
Spray booth absolutely necessary as you don't want the aerosol paints drifting through your studio contaminating every surface.

Gee I can't understand why I got devitrification......
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: enamel suggestions

Post by peter cummings »

Thanks Kevin. More experiments, when the switches are replaced. Why do I get too many ideas?
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: enamel suggestions

Post by Don Burt »

The application technique probably matters more than the paint if you're going for a watercolor look. If you want brilliant transparent color, you're limited to lead bearing low fire enamels. Airbrushing those paints is a challenge in managing overspray and cleanup, but some crazy people do it. Email for details. But watercolor pigment on paper isn't optically transparent...it's just as opaque as any glass paint, but it is applied thinly on bright white paper. To work in less optically clear paints with airbrush, you can use any of the powdered glass paints: Sunshine, Fusemaster, Reusche, whatever. I mix the paint with a weak liquid gum mixture (klyrfire?...I can never remember how they spell it) and isopropyl alcohol. But here's the thing....I airbrush largish areas sometimes with lots of different paint, and none of it ever looks 'watercolor'-like. The low-fires can look slick and jewel like, and there's some edge blending of color borders if enough is applied, but it normally fires to look more like canned spray paint or nail polish. You can better get wash-like overlap and edge seeping with brush applied paint using oil-based mediums. China painters do it all the time. Lavender oil, water-friendly oil mediums, traditional oil painting mediums...stuff like that. If you google Guy Kemper Glass Art and look at his stuff, he gets some water color effects, but he's working huge scale. He also usually has the infrastructure and staff of Derix studio in Germany helping him: rooms dedicated to spraying, acid etching sheets of flashed Lamberts, laminating sheets....big stuff. But I think China painting technique might be the way to go. Paul Lewing's book on china painting is good. The best book on oil painting mediums ever is Gene Patterson's 'Book for the Curious Painter'. Gene passed away and the book was out of print for a while, but some china painting people have started republishing it. I refer to it still from time to time.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: enamel suggestions

Post by Kevin Midgley »

Don suggested "some crazy people".
An alternative to paint that could drive you crazy would be to use sheets and powders of tint glass layered and also sand blasted thinner so as to change the colour densities.
Guaranteed to be difficult and drive you crazy in the process but probably no more than trying to keep your studio clean from air brushing enamels.
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: enamel suggestions

Post by Terry Gallentine »

I have done work very similar to wet on wet watercolor by sandblasting the glass first for tooth. Then load the sandblasted glass with water and start to paint on the enamels. The flow that I got was very similar to watercolor washes.
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: enamel suggestions

Post by peter cummings »

Thanks everyone. An update in case you think I gave up. I checked out what's available and researched them. I tried the a very low temp enamel which came lose when I engraved it afterwards. Usual fused glass powders worked out expensive and not the way to go. Having loose release powder under made a rough surface which is no good for engraving, impossible to get a good edge. I'm nearly there with Fusemaster high fire enamels and just bought an airbrush to get a thinner smoother surface. I don't mind the brush strokes and thinner will let more light through. Also today the fusemaster transparent enamels arrived to try. Nearly there he says. I'll put a photo in that section.
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: enamel suggestions

Post by Don Burt »

Airbrushing fusemaster transparents: one of the most effective techniques for introducing lead monosilicate into your studio atmosphere. I do it all the time (not with fusemaster, but their equivalent). Be careful Peter please.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: enamel suggestions

Post by Kevin Midgley »

Do air brushing inside a spray booth with supreme filtration at the exit end of that filter. Air brushing will suspend particles in the air for Hours and hours after spraying.
Please visualize a brilliantly sunny day where a beam of sunlight comes inside your room and you can see the 'house dust' drifting around. Now visualize even smaller breathable particles of paint drifting in that same air. Clouds of it. :shock:
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: enamel suggestions

Post by DonMcClennen »

I was able to get a watercolour look by mixing powder frit with "cable pull gel" (available at Home Depot) You wind up with a acrylic paint like consistency. Then apply to glass with brushes as if painting a watecolour . try it !!
"The Glassman"
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: enamel suggestions

Post by peter cummings »

Now I might stick with brushes, it's a bit of a worry. Been using opaques, and just got transparents. Maybe I can fix up a booth, temp. cause I'm running out of room. I've started writing all the steps I've been through so far and will put them on my blog soon. Thanks for advice. I wish I had a glass community closer but regularly thank the internet.
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: enamel suggestions

Post by Don Burt »

DonMcClennen wrote:I was able to get a watercolour look by mixing powder frit with "cable pull gel" (available at Home Depot) You wind up with a acrylic paint like consistency. Then apply to glass with brushes as if painting a watecolour . try it !!
Got any idea what it is, from a chemical standpoint, Don? I’ve tried gel baby oil and didn’t get anywhere with it
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: enamel suggestions

Post by DonMcClennen »

Container says: Clear Glide wire pulling lubricant by IDEAL #31-388.. maybe you can find it online. When fire it left some texture. Don
"The Glassman"
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: enamel suggestions

Post by Kevin Midgley »

I reckon all the gels used to thicken or stick stuff are just variations of all the different gums you can get that can be used to prepare food.
The last one I made, didn't stick glass together all that well but I'd made a very liquid batch of guar gum in a tiny plastic eye drops empty bottle. I put a few granules of gum into the bottle, shook it up and put it in the microwave for a few seconds. Wanted to squirt everywhere from the heating, but it burned out clear. Next batch I'll add more granules and microwave for less time.
If you are making a large batch and don't want it to go bad, add a few drops of bleach to the mixture. Probably easier to make your own than find something from North America in Australia. By the time you have to test the stuff after you have found it, you may as well make your own and test that.
Unlike wanting to use a brush to apply the gel, I have trouble find small enough bottles with droppers that don't flood my glass.
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: enamel suggestions

Post by peter cummings »

Well I made a small spray booth, by up ending a 3 ft table and closing most of it in. Arm holes and extractor port as well. If I take glass top off I can just up end again to use as a table. Going to look for gum stuff, food or "clear glide wire pulling lubricant" sounds like a fun thing to ask for in engineering shops around here. No experimenting today as there's a heat wave inc. bad winds and serious fire problems just up the highway where I know people. I will put our animals on glass soon, because that may be the only way we can see or remember them the way it's going.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: enamel suggestions

Post by Buttercup »

Peter, a used appliance box, such as a TV or microwave box, with appropriate holes cut in it and a strong extractor fan makes a good spray booth that can be flat-packed for easy storage when not in use.

Take care with these terrible bushfires. Jen
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: enamel suggestions

Post by Kevin Midgley »

Not engineering shops but electrical installers.
Those food grade gums since they make water thicker and into a gel, are good for putting on burns or fires for that matter.
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: enamel suggestions

Post by peter cummings »

Airbrush isn't too difficult, gives a much thinner layer. I'm going to try gum arabic as a dilutant, and maybe glycerine which will certainly make it goooey. The plan is working out ok though. I'm going to try a photo in pictures section now. Thanks all. Smokey here but the fires are up in the hills an hour away.
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: enamel suggestions

Post by jim burchett »

You could try clear aloe gel that you can find it burns off cleanly.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: enamel suggestions

Post by Buttercup »

Hi Peter,

Did you ever find the cable-pulling gel? Here's a link to an Oz company that advertises it:

https://www.specialisedforce.com.au/pro ... -lubricant

They seem to be in every major city with products probably distributed all over the country.

WARNING: A different company's Google listing came up just after it. When I clicked on that Firefox warned me not to proceed as it is an insecure site.

Let us know how it goes if you try it.
Post Reply