The glass that I purchase has a lot of micro bubbles and often folds, when I make beads I really don't want bubbles, but Even with a 20 minute bubble squeeze still has bubbles.
ify beads 12mm to 18mm size, have bubbles will a fire polish/ or fuse again and add a longer bubble squeeze of maybe 60. minutes will that remove pre existing bubbles
bubbles
Moderator: Tony Smith
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: bubbles
I am sorry to inform you that if these are "micro"bubbles, then you are stuck with them unless you can figure
out a way to remelt the glass and hold for a long time.
The other Jim
out a way to remelt the glass and hold for a long time.
The other Jim
-
- Posts: 128
- Joined: Sun Jun 08, 2003 5:27 pm
- Location: East Tennessee
Re: bubbles
Bullseye considers the micro bubbles a "feature" of the handmade glass aspect. I think they also consider the "runs" on the top surface the same, but those certainly cause me a lot of problems when trying to match the gradient in dichroic glass.
Lynn Perry