Norton drywall screen for removal of kiln wash

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Kelly & Charlie MacMu

Norton drywall screen for removal of kiln wash

Post by Kelly & Charlie MacMu »

Thanks AVLucky!! It took probably less than 2 minutes to clean off 3 kiln shelves. I had a respirator on ( lots of dust ) great Idea :lol: The stuff cost about $10.00 for ten sheets of it.

( Norton h20 proof 120 grit sand paper available at homedepot)
AVLucky
Posts: 74
Joined: Fri Jan 30, 2004 6:15 pm
Location: PA

Post by AVLucky »

You're welcome.

I love that stuff. It's a real lifesaver.
Post Reply