Working Deep MESS

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Post by Barbara Muth »

Jackie Beckman wrote:
BTW Jackie, I liked your experiment. Another try to push out some of the bubbles and I think you will have something quite nice.

Phil
Thanks Phil. I'm anxious to try the one I build face down. I think with the strips being at the face, so that I can blast and texture them, then the imagery being at the very back, it may be something interesting. (Everyone really should have their very own Cindy-Next-Door to discuss these things with!) And now that I know I can fire it for less that the cost of a Venti Latte, I'll give it a shot. Thanks! :)
I like that idea a lot Jackie. Having your dancing texture beneath a lens of clear glass could do interesting things for it. Can't wait to see more!

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS
Post Reply