I use Spray A now and then with a few of my pickier opals. Although eliminating Thinfire has helped with my devit problem.

I did some tack fused ornaments recently and used Spray A to 1325°. My ornaments were all splotched and looked like they'd been sprayed. I've made the mistake before; in my opinion, Spray A has to be fired over 1400° to fully melt into the glass.