Pre-Cut Letters and Numbers

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Lia Howe
Posts: 40
Joined: Tue Mar 18, 2003 1:36 pm
Location: Haliburton, Ontario

Pre-Cut Letters and Numbers

Post by Lia Howe »

Does anyone know where to get 90 C.O.E cut out letters and numbers. Small ones. 1 to 3 inch. Bullseye would be my glass of choice but Uros is okay too. I have a ring saw and I cut my own but I heard someone talk about Water Jet cut shapes. This would probably be easier but I can't buy anymore equipment. Anyone know if these are availiable anywhere?Lia
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Re: Pre-Cut Letters and Numbers

Post by Ron Coleman »

Lia Howe wrote:Does anyone know where to get 90 C.O.E cut out letters and numbers. Small ones. 1 to 3 inch. Bullseye would be my glass of choice but Uros is okay too. I have a ring saw and I cut my own but I heard someone talk about Water Jet cut shapes. This would probably be easier but I can't buy anymore equipment. Anyone know if these are availiable anywhere?Lia
There was a post about this a few weeks back. Here's a link to the info.
http://www.warmglass.com/phpBB/viewtopi ... ht=letters

Ron
Harry
Posts: 13
Joined: Fri Mar 14, 2003 2:19 am
Location: Portland OR

Post by Harry »

WE would be happy to cut letters or numbers for you. Please give us a call for a quote. Waterjet Design Hillsboro OR 503-615-0144
Post Reply