FABRIC FIRING?

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
Ann Demko
Posts: 104
Joined: Mon Mar 10, 2003 11:54 pm
Location: Owensboro, KY

FABRIC FIRING?

Post by Ann Demko »

Just viewed the rest of Patty Grays pics and have a question on the fabric firing. Does one just take the piece to tack fuse in order to not lose the texture of all those cute litle stringers? Then can you slump the piece and it would stay altogether? Ann Demko
The Hobbyist
Posts: 308
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Post by The Hobbyist »

Yes and yes................Jim
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Post by jim simmons »

To echo Jim, Yes...and Yes..... Also, remember that they probably will not be water tight :cry:

The "other" Jim
Patty Gray
Posts: 70
Joined: Mon Mar 10, 2003 9:47 pm
Location: Washington
Contact:

Post by Patty Gray »

You can make it water tight if you use a sheet of glass on the surface which will become the inside of the piece. That isn't the way I normally did the process but I did at times for certain individuals. The ones that Corning bought were completely stringer.

It's just a tad more than a tack fuse and the pattern is on the underside which becomes the outside.

Have fun,

Patty Gray
time4sun@worldnet.att.net
http://www.pattygray.com