Cutting pattern bars
Posted: Fri Jul 18, 2003 10:35 am
by michelle andre
I have been trying to cut a pattern bar ( approx. 1"x1") with a tile saw that has a 8" diamond wheel. The cut seems to go well until the last bit where a chunk of the the bar breaks off and leaves a nub on the pattern tile I have just cut. Does anyone have any suggestions on how I might achieve a clean uniform cut?
Posted: Fri Jul 18, 2003 11:25 am
by Robin Z
When you get to the end of the cut you need to slow down to a crawl.
Posted: Fri Jul 18, 2003 12:14 pm
by Terry Ow-Wing
another trick is when you create the pattern bar put clear all around the "pattern" that way when chip outs do occure you are not losing the actual pattern. good luck.
-Terry O.
Posted: Fri Jul 18, 2003 2:07 pm
by Brock
Rotate your block so that you are always cutting towards the center. Another good tip is to NEVER put white glass on the outside edges of a pattern bar, it's so hard it almost always chips. Brock